Abstract
The hydrothermal reaction of KVO3, PhPO3H2 and water at 180°C for 116 h yields the tubular mixed valence Vv/Viv polymer (H3O)[(V3O4)(H2O) (PhPO3)3]·xH2O (x = 2.33).